Design basis for bauxite wet tropical climate
The design basis starts with the rock, not the machine. Bauxite is rated at 30–90 MPa compressive strength with low abrasiveness, high moisture sensitivity and a loose bulk density around 1.35 t/m³. Sticky, clay-rich feed blocks grizzlies and screens; wet processing and generous transfer chutes are usual. Record the setting before adjusting it, or the baseline is lost.
A wet tropical climate must keep screening reliable through a long rainy season, constrained by high feed moisture and clay-bearing overburden. The commercial priority is wet screening and washing. For this combination HAMAC works from an indicative design point of 150 t/h of saleable product, with a maximum feed top size near 350 mm and target fractions of sized ore and washed fines.
| Parameter | Indicative value / method |
|---|---|
| Raw material | Bauxite · 30–90 MPa · abrasion low |
| Design throughput | 150 t/h saleable product (120–300 t/h scenario band) |
| Maximum feed size | ~350 mm |
| Target product | sized ore and washed fines |
| Loose bulk density | 1.35 t/m³ |
| Suggested circuit | impact crusher → washing screen |

Why clay contamination appears in this circuit
Screens blind and the chamber packs during wet weather. In a bauxite wet tropical climate this is usually a system symptom rather than a single machine fault. A supplier can only guarantee a figure when the test conditions are written down.
- clay-bearing overburden enters with the shot rock
- spray water is added without a washing circuit
- transfer chutes are too narrow for sticky material
Indicative values are starting points for a design, not guarantees. Before changing a crusher setting, check these in order: 1) measure surface moisture at the shift level; 2) inspect deck open area after each wet shift; 3) log the pressure drop across dust collection. Agree the acceptance test and sampling method before the order is placed.
Recommended equipment configuration
For bauxite at 150 t/h the working train is impact crusher → washing screen. The equipment list is fixed only after feed gradation, moisture and saleable fractions are confirmed — the same nominal capacity can require different crushers for bauxite and for a softer rock. Record the setting before adjusting it, or the baseline is lost.
| Parameter | Indicative value / method |
|---|---|
| Feeding | Vibrating grizzly feeder, VFD control, ~188 t/h design margin |
| Primary reduction | Jaw / impact crusher, nominal CSS ~18 mm at the secondary stage |
| Secondary / tertiary | washing screen |
| Screening | Multi-deck screen sized for 50% circulating load |
| Conveying | Belts sized for fresh feed + return stream, 1.35 t/m³ bulk density |
| Control | Interlocked start-up, power-based feed trim, 410 kW order-of-magnitude connected load |
The corrective actions for clay contamination are applied on top of this base circuit: scalp clay at the grizzly before primary crushing; choose rubber or polyurethane media with ball trays; add a washing stage with water recovery where the specification allows.

Operating settings and acceptance checks
Settings must be recorded at commissioning and re-checked after every liner change. For this circuit the starting point is a secondary CSS near 18 mm, a circulating load around 50% and a screen efficiency target above 90%. Indicative values are starting points for a design, not guarantees.
- Measure surface moisture at the shift level
- Inspect deck open area after each wet shift
- Log the pressure drop across dust collection
| Parameter | Indicative value / method |
|---|---|
| Capacity | Measured over a full shift, saleable tonnes, 150 t/h nominal |
| Grading | Full sieve analysis, agreed standard, sized ore and washed fines |
| Crusher setting | CSS measured and logged, ~18 mm starting point |
| Power | Main-drive current at steady feed, 410 kW connected load |
| Wear | Liner mass before and after, cost per saleable tonne |
Agree the acceptance test and sampling method before the order is placed. All figures published on this site are nominal engineering values; actual performance depends on feed gradation, moisture, crusher setting and screening efficiency.
Cost, risk and what to confirm in writing
Compare this plant as cost per saleable tonne, not purchase price. Energy, wear parts, labour and downtime dominate the operating cost for bauxite, while wet screening and washing determines how much lost production actually costs. A supplier can only guarantee a figure when the test conditions are written down.
- Ask every supplier for the same flow sheet and mass balance, including the 50% return stream.
- State the Incoterm, named port, civils scope, erection scope and a two-year spares list in the quotation.
- Model annual output as 150 t/h × scheduled hours × realistic utilisation (often 75–90%), not as nameplate × 8,760 hours.
- Agree the sampling method, sieve standard and acceptance test before the order is placed.
Record the setting before adjusting it, or the baseline is lost. Agree the acceptance test and sampling method before the order is placed. Send your material, feed size, target capacity and product sizes to HAMAC Machinery for a comparable configuration and budget.