Overview
A bauxite crushing plant turns raw bauxite into graded aggregate, ore feed or industrial mineral. Material properties — Mohs 2, compressive strength ~50 MPa, low abrasion — decide the circuit.

Bauxite material profile
| Property | Value |
|---|---|
| Mohs hardness | 2 |
| Compressive strength | 50 MPa |
| Abrasion | Low |
| Recommended circuit | jaw + impact |
Recommended circuit
HAMAC configures Bauxite plants as: jaw + impact. Washed and screened, then refined to alumina.
Typical equipment
- PE Series Jaw Crusher — Jaw crushers are often used for primary crushing in mine material crushing.
- PF Impact Crusher — The impact crusher (impact crusher) is a new generation of impact crusher developed in com
- Vibrating Screen — The YK Series Circular Vibrating Screen is designed for screening various ores and buildin
Capacity range
From 30 t/h contractor units to 1,000+ t/h quarry lines, with multi-deck screening for several saleable fractions.
Reference data for this configuration
| Parameter | Reference value |
|---|---|
| Feed material | Bauxite |
| Mohs hardness | 2 |
| Compressive strength | ~50 MPa |
| Abrasiveness | Low |
| Recommended circuit | jaw + impact |
| Assumed duty | mine pre-beneficiation feed |
| Evaluation horizon | five-year view |
The figures above are transcribed from published HAMAC data and from the material properties of bauxite; site measurements take precedence.
Project profile these notes assume
| Assumption | Value |
|---|---|
| Operating duty | mine pre-beneficiation feed |
| Primary objective | maximum mechanical availability |
| Evaluation horizon | five-year view |
| Site condition | a greenfield site |
| Operating team | a rotating shift crew |
Change any one of these assumptions and the recommended configuration for bauxite crushing may change. HAMAC re-runs the same checks against your own numbers once the enquiry data sheet is received.
From enquiry to the first saleable tonne
- Book shipping, prepare the packing list and confirm the container loading plan.
- Verify the electrical single-line diagram, cable sizing and starter type with the local utility.
- Plan training for a rotating shift crew on CSS adjustment, liner change-out and lock-out / tag-out.
- Define the acceptance test: sampling points, test duration, moisture range and who signs the protocol.
- Apply jaw + impact; the reduction mechanism must suit low abrasion and a compressive strength near 50 MPa.
- Commission with graded load, sample the product grading, then train operators on liner change-out and daily checks.
- Check bearing and lubrication arrangements against the ambient temperature range at the site.
- Review the crusher chamber profile with the liner supplier against Bauxite (Mohs 2, ~50 MPa, low abrasion).
- Include dust suppression, guarding, emergency stops and lock-out points in the layout drawing.
Most delays at this stage come from missing feed data rather than from manufacturing capacity.

What to verify before you sign
- Written performance guarantee, sampling method and acceptance-test protocol.
- Decommissioning or relocation value at the end of a five-year horizon.
- Wear-part interchangeability across machines in the same circuit.
- Closed-side setting range and whether automatic setting regulation is included.
- Spare motor, gearbox and hydraulic pump lead times from the nearest HAMAC stock point.
- After-sales response time, technician availability and the warranty exclusions in writing.
- Product sampling points and the lab equipment needed for routine grading checks.
- Liner alloy: Mn18 with ceramic inserts is a common starting point for bauxite at low abrasion.
- Maximum feed lump and gradation — a chamber that cannot accept the top size will bridge on day one.
Score each supplier against the same ten items and keep the score sheet with the purchase file for the five-year review.
Where the money actually goes
| Cost line | Indicative share | What moves the number |
|---|---|---|
| Equipment & drive packages | 55% | Model size, number of stages and automation level |
| Ocean freight & insurance | 8% | Destination port, container count and out-of-gauge cargo |
| Civil works & foundations | 8% | Soil conditions, dynamic loads and site preparation |
| Erection, commissioning & training | 7% | Local labour, supervision scope and schedule |
| First-year wear parts | 14% | Rock abrasiveness, liner grade and operating hours |
| Power, lubricants & consumables | 8% | kWh per tonne, local tariff and dust suppression water |
Include downtime in the model. An unplanned liner change on a remote site costs far more than the casting itself.
Mistakes that cost more than the machine
- Buying maximum mechanical availability on price alone and losing it in availability.
- Choosing screen apertures before the concrete or asphalt mix design is fixed.
- Leaving tramp-iron protection out of the scope to save a small percentage of capital.
- Using one liner profile for both secondary and tertiary stages.
- Forgetting surge capacity — an intermittent loader starves the chamber and ruins particle shape.
- Buying on nameplate t/h without converting to saleable product at the specified fractions.
- Skipping a geotechnical check and discovering settlement under the primary crusher at a greenfield site.
- Specifying motors for the wrong voltage or frequency and rewinding them on site.
Review the list with a rotating shift crew before the order is placed — they will recognise most of them.
Commissioning checklist
- Calibrate the belt scale and any level probes against a known load.
- Agree the punch list, sign the hand-over protocol and file the as-built drawings.
- Measure and log the as-new CSS / setting for future wear comparison.
- Sample each product fraction and compare with the specification.
- Check belt tracking, chute build-up and transfer-point dust.
- Check hydraulic pressure, accumulator pre-charge and tramp-release function.
- Introduce feed in graded steps: 25%, 50%, 75%, then full load.
- Record the baseline grading curve for each product fraction.
Keep the signed record; it is the only defensible baseline for later performance disputes.